Production process of worsted high count yarn camel hair product

文档序号:1283249 发布日期:2020-08-28 浏览:39次 中文

阅读说明:本技术 一种精纺高支纱驼绒制品生产工艺 (Production process of worsted high count yarn camel hair product ) 是由 李智善 何睿 于 2020-04-02 设计创作,主要内容包括:本申请公开了一种精纺高支纱驼绒制品生产工艺,包括以下步骤:S1:驼绒预处理,将驼绒进行除尘、水洗、风干、分梳;S2:编织坯布,将预处理好的驼绒放入针织大圆机中编织;S3:高温洗缩,将编织好的坯布放入高温机缸中进行高温水洗,水洗接收胡放入加绒起助剂和柔软助剂烘干;S4:起绒整理,将整理好的坯布由24针辊的起绒机起绒,所述起绒机的张力由轻到重,直至将驼绒毛根拉散成为绒状为止。S5:起绒后整理,将起绒好的坯布用36针辊5的舒绒机梳理顺畅,随后根据实际需要的克重和门幅在定型机上定型。本申请的一种精纺高支纱驼绒制品生产工艺生产的驼绒制品经纱:36S/2,纬纱36S/2,平方米克重:290g,宽幅:180㎝,无异味。(The application discloses worsted high count yarn camel hair product production technology, including the following steps: s1: preprocessing camel hair, and performing dust removal, water washing, air drying and carding on the camel hair; s2, weaving gray fabric, namely, putting the pretreated camel hair into a circular knitting machine for knitting; s3: washing and shrinking at high temperature, namely putting the woven grey cloth into a high-temperature machine cylinder for high-temperature washing, and putting the washed receiving urheen into a fluffing assistant and a softening assistant for drying; s4: and (3) napping finishing, namely napping the finished grey cloth by a napping machine with 24 needle rollers, wherein the tension of the napping machine is changed from light to heavy until the camel hair roots are scattered into a napped state. S5: and (3) finishing after napping, namely carding the napped grey cloth smoothly by using a napping machine with 36 needle rollers 5, and then shaping on a shaping machine according to the gram weight and the width of the fabric required actually. The camel hair product produced by the worsted high count yarn camel hair product production process has the warp of 36S/2, the weft of 36S/2 and the square meter gram weight: 290g, width: 180 cm, no peculiar smell.)

1. A production process of a worsted high count yarn camel hair product is characterized in that: the method comprises the following steps:

s1: preprocessing camel hair, and performing dust removal, water washing, air drying and carding on the camel hair;

s2, weaving gray fabric, namely, putting the pretreated camel hair into a circular knitting machine for knitting;

s3: high-temperature washing and shrinking, namely placing the woven grey cloth into a high-temperature machine cylinder for high-temperature washing, and placing the wool raising auxiliary agent into a washed receiving urheen

And drying the mixture with a softening auxiliary agent;

s4: raising and finishing, raising the finished grey cloth by a 24-needle roller raising machine until the grey cloth is raised to a required level

The camel hair root is pulled to be dispersed into a velvet shape.

S5: and (3) finishing after napping, namely carding the napped grey cloth smoothly by using a napping machine with 36 needle rollers 5, and then shaping on a shaping machine according to the gram weight and the width of the fabric required actually.

2. The process for producing a worsted high count camel hair product as claimed in claim 1, wherein: in the step S1: the camel hair is MC1 camel hair, the average length is more than 45mm, the average diameter is less than 17.3 microns, and the content is less than 2%.

3. The process for producing a worsted high count camel hair product as claimed in claim 1, wherein: in the step S1, the camel hair is decolorized at a low temperature, and a wool protective agent is added during the treatment.

4. The process for producing a worsted high count camel hair product as claimed in claim 1, wherein: in the step S5, the working temperature of the setting machine is 150 ℃.

Technical Field

The application relates to the technical field of camel hair product preparation, in particular to a production process of a worsted high count yarn camel hair product.

Background

Disclosure of Invention

The invention aims to provide a production process of a worsted high count yarn camel hair product, which overcomes the defects in the prior art.

In order to achieve the purpose, the invention provides the following technical scheme: a production process of a worsted high count yarn camel hair product comprises the following steps:

s1: preprocessing camel hair, and performing dust removal, water washing, air drying and carding on the camel hair;

s2, weaving gray fabric, namely, putting the pretreated camel hair into a circular knitting machine for knitting;

s3: high-temperature washing and shrinking, namely placing the woven grey cloth into a high-temperature machine cylinder for high-temperature washing, and placing the wool raising auxiliary agent into a washed receiving urheen

And drying the mixture with a softening auxiliary agent;

s4: raising and finishing, raising the finished grey cloth by a 24-needle roller raising machine until the grey cloth is raised to a required level

The camel hair root is pulled to be dispersed into a velvet shape.

S5: and (3) finishing after napping, namely carding the napped grey cloth smoothly by using a napping machine with 36 needle rollers 5, and then shaping on a shaping machine according to the gram weight and the width of the fabric required actually.

Preferably, in step S1: the camel hair is MC1 camel hair, the average length is more than 45mm, the average diameter is less than 17.3 microns, and the content is less than 2%.

Preferably, in step S1, the camel hair is decolorized at a low temperature, and a wool protective agent is added during the decolorization.

Preferably, in step S5, the working temperature of the setting machine is 150 ℃.

Compared with the prior art, the production process of the worsted high count yarn camel hair product has the advantages that the warp yarn of the camel hair product produced by the production process is 36S/2, the weft yarn is 36S/2, and the square meter gram weight: 290g, width: 180 cm, no peculiar smell.

Detailed Description

Technical solutions in the embodiments of the present invention will be described in detail below, and it is apparent that the described embodiments are only a part of the embodiments of the present invention, and not all embodiments. All other embodiments, which can be obtained by a person skilled in the art without any inventive step based on the embodiments of the present invention, are within the scope of the present invention.

The production process of the worsted high count yarn camel hair product is selected as follows: component MC1 camel hair; the fineness is less than or equal to 17.3 um; the length is more than or equal to 45mm, and the content is not more than 2%. Firstly, a carding process is carried out on the raw materials, and the carding process flow comprises the following steps:

half of the raw material needs to be decolorized because the camel hair raw material is purple-white interweaved. Because the raw materials are greatly damaged by decoloring, low-temperature decoloring is adopted, and a wool protective agent is added in the decoloring process.

Combing camel lambs wool → making strip → spinning → weaving of circular knitting machine → inspection → repairing → washing shrinkage → raising wool → combing wool → shearing → shaping → finished product

Weaving gray fabric: material 12SThe gray fabric is woven by a 30-34 inch, 19-24 needle cylinder and a circular knitting machine with a sinker height of 1.8-3.5 wool (determined according to different widths, gram weights and fabric styles). The loss of the camel hair in the working procedure is about 3 percent.

Washing and shrinking: and (3) washing the woven grey cloth in a high-temperature machine cylinder at high temperature, adding a raising auxiliary agent and a softening auxiliary agent, drying and then entering the next raising process.

Raising and finishing: the finished color blank is napped by a napping machine with 24 needle rollers, and the camel hair ring is broken by a continuous 6-machine under the tension of light weight until the broken camel hair roots are scattered into a napped state.

Carding and finishing: carding the scattered velvet with the cloth cover smoothly by using a velvet loosening machine with 36 needle rollers 5, and combing the flat velvet to be vertical, wherein the velvet is to be combed to the bottom.

Shearing and finishing: according to the suede style of the camel hair fabric, redundant floating hair is cut off, so that the suede is flat, and the suede height is consistent.

And (3) shaping and finishing, namely stabilizing the texture structure of the fabric on a shaping machine at a temperature of about 150 ℃ according to the actual required gram weight and width to meet the actual required requirements.

In summary, the production process of the worsted high count yarn camel hair product has the advantages that the warp yarn is 36S/2, the weft yarn is 36S/2, and the square meter gram weight: 290g, width: 180 cm, no peculiar smell.

It is noted that, herein, relational terms such as first and second, and the like may be used solely to distinguish one entity or action from another entity or action without necessarily requiring or implying any actual such relationship or order between such entities or actions. Also, the terms "comprises," "comprising," or any other variation thereof, are intended to cover a non-exclusive inclusion, such that a process, method, article, or apparatus that comprises a list of elements does not include only those elements but may include other elements not expressly listed or inherent to such process, method, article, or apparatus. Without further limitation, an element defined by the phrase "comprising an … …" does not exclude the presence of other identical elements in a process, method, article, or apparatus that comprises the element.

The foregoing is merely a detailed description of the present application, and it should be noted that modifications and embellishments could be made by those skilled in the art without departing from the principle of the present application, and these should also be considered as the protection scope of the present application.

4页详细技术资料下载
上一篇:一种医用注射器针头装配设备
下一篇:一种芳香型耳带及其制作方法

网友询问留言

已有0条留言

还没有人留言评论。精彩留言会获得点赞!

精彩留言,会给你点赞!