Efficient collecting agent for collecting copper and gold from copper smelting slag and preparation method thereof

文档序号:1162414 发布日期:2020-09-18 浏览:15次 中文

阅读说明:本技术 一种从铜熔炼渣中捕收铜、金的高效捕收剂及其制备方法 (Efficient collecting agent for collecting copper and gold from copper smelting slag and preparation method thereof ) 是由 田晓东 谢兰馨 赖春华 翁存建 王鹏程 冯媛媛 于 2020-05-25 设计创作,主要内容包括:本发明公开了一种从铜熔炼渣中捕收铜、金的高效捕收剂及其制备方法,其配方包括,二硫代磷酸盐15%~20%、磺酸15%~25%、氯乙酸钠20%~30%、黄原酸盐20%~30%、烷胺20%~30%、N,N-二甲基甲酰胺5%~15%。本发明通过利用不同结构、不同类型捕收剂之间的构效关系以及协同效应,使捕收能力较强的分子吸附在矿物表面活性较弱的吸附位点,而捕收能力较弱的分子吸附在矿物表面活性较高的吸附位点,从而使矿物表面吸附更多的捕收剂分子,实现了铜熔炼渣中铜、金的高效综合回收,避免了有价金属的损失和其对环境的污染,同时带来经济效益。相对于改进浮选流程及设备,本发明使用常见的化合物进行复配即可制得,可极大地节省人力物力。(The invention discloses a high-efficiency collector for collecting copper and gold from copper smelting slag and a preparation method thereof, wherein the formula comprises 15-20% of dithiophosphate, 15-25% of sulfonic acid, 20-30% of sodium chloroacetate, 20-30% of xanthate, 20-30% of alkylamine and 5-15% of N, N-dimethylformamide. According to the invention, through utilizing the structure-activity relationship and synergistic effect among different types of collectors with different structures, molecules with stronger collecting capacity are adsorbed on adsorption sites with weaker activity on the surface of the mineral, and molecules with weaker collecting capacity are adsorbed on adsorption sites with higher activity on the surface of the mineral, so that more molecules of the collectors are adsorbed on the surface of the mineral, the high-efficiency comprehensive recovery of copper and gold in copper smelting slag is realized, the loss of valuable metals and the pollution of the valuable metals to the environment are avoided, and meanwhile, the economic benefit is brought. Compared with the improved flotation process and equipment, the invention can be prepared by compounding common compounds, and can greatly save manpower and material resources.)

1. The utility model provides a high-efficient collector of collecting copper, gold in follow copper smelting sediment which characterized in that: the code of the high-efficiency collector is XK-419, and the formula comprises: the compound fertilizer comprises dithiophosphate, sulfonic acid, sodium chloroacetate, xanthate, alkylamine and N, N-dimethylformamide, and the raw materials in percentage by mass are as follows: 15 to 20 percent of dithiophosphate, 15 to 25 percent of sulfonic acid, 20 to 30 percent of sodium chloroacetate, 20 to 30 percent of xanthate, 20 to 30 percent of alkylamine and 5 to 15 percent of N, N-dimethylformamide.

2. A high efficiency collector for collecting copper and gold from copper smelting slag according to claim 1, which is characterized in that: the dithiophosphate is composed of at least one of dibutyl dithiophosphate, diisobutyl dithiophosphate, di-n-amyl dithiophosphate and diisoamyl dithiophosphate.

3. A high efficiency collector for collecting copper and gold from copper smelting slag according to claim 1 or 2, wherein: the sulfonic acid is composed of at least one of taurine, benzenesulfonic acid, sulfamic acid, ethanesulfonic acid, sodium benzenesulfonate and pyridine-2-sulfonic acid.

4. A high efficiency collector for collecting copper and gold from copper smelting slag according to claim 1, which is characterized in that: the xanthate is composed of at least one of sodium ethyl xanthate, sodium n-butyl xanthate, sodium isobutyl xanthate, sodium n-pentyl xanthate, sodium isopentyl xanthate and sodium sec-octyl xanthate.

5. A high efficiency collector for collecting copper and gold from copper smelting slag according to claim 1, which is characterized in that: the alkylamine is composed of at least one of ethylamine, propylamine, n-butylamine, isobutylamine, n-pentylamine, isopentylamine, p-phenylenediamine, o-phenylenediamine, 1, 2-propylenediamine, 1, 6-hexamethylenediamine, 1, 4-butylenediamine and 1, 5-naphthalenediamine.

6. A high efficiency collector for collecting copper and gold from copper smelting slag according to claim 1, which is characterized in that: the mass fraction of the dithiophosphate is 15%, the mass fraction of the sulfonic acid is 15%, the mass fraction of the sodium chloroacetate is 20%, the mass fraction of the xanthate is 20%, the mass fraction of the alkylamine is 20%, and the mass fraction of the N, N-dimethylformamide is 10%.

7. The preparation method of the efficient collector for collecting copper and gold from copper smelting slag according to claim 1 is characterized in that: firstly, weighing the raw materials in proportion, then placing sodium chloroacetate in a container, adding N, N-dimethylformamide, slowly adding xanthate while stirring, and stirring and reacting in a constant-temperature water bath at 80 ℃ for 2 hours; when the temperature is reduced to 20-30 ℃, slowly dripping alkylamine into the container, and stirring for 1 hour at the constant temperature of 50 ℃; and finally, slowly adding dithiophosphate and sulfonic acid in sequence, and uniformly stirring to obtain the high-efficiency collector XK-419.

Technical Field

The invention relates to the technical field of non-ferrous metal mineral separation, in particular to a collecting agent for efficiently collecting copper and gold from copper smelting slag and a preparation method thereof.

Background

Pyrometallurgical copper smelting is one of the main methods for copper smelting, and a large amount of smelting waste slag is generated in the smelting process, and a large amount of valuable metals are contained in the smelting waste slag. If the stacking is directly carried out, not only is the resource waste caused. Meanwhile, heavy metal ions contained in the smelting slag can be brought into underground water by precipitation, and serious influence is caused on the environment. Therefore, how to recycle valuable metals in the part of smelting waste residue is always a difficult point of current research.

Studies by Chenghuanliang et al report a process for comprehensively recovering copper and iron from a certain copper smelting slag (reference: Chenghuanliang, Liuzhanhua, Dingyinobao, Cao Shi Cheng. In this process, Z-200 is used as a collector. Through a closed flow of secondary roughing, primary scavenging and secondary concentration, the recovery rate of Cu in the concentrate is finally 87.81%. However, the use of Z-200 flotation for the existing copper smelting slag is less effective. Renyanhua et al also studied a beneficiation process of a certain copper smelting slag to recover copper in 2019 (reference: Renyanhua, Zhanming, Guokong, Kong, Welliang, Liyunpeng. a beneficiation process test of a certain copper smelting slag to recover copper [ J ] research and development of mining industry, 2019,39(03):63-66.), and used KM-109 as a collector in the flotation process at an amount of 300 g/t. Finally, the recovery rate of the Cu rough concentrate in the copper smelting slag reaches 79.77 percent through a closed flow of primary roughing, secondary refining and sweeping. However, the KM-109 collector used in the research is too high in dosage, so that the treatment cost is high. Therefore, in order to avoid the waste of valuable metals in the copper smelting slag and the pollution to the environment, the collecting agent which takes the copper smelting slag as a research object so as to effectively collect copper and gold from the copper smelting slag has important significance for treating the copper smelting slag in a smelting plant.

Disclosure of Invention

The invention aims to solve the technical problem that the existing copper smelting slag has poor Z-200 flotation effect, and provides a novel collecting agent for efficiently collecting copper and gold from the copper smelting slag and a preparation method thereof. The collector has strong collecting capacity for Cu and Au, and has efficient foaming performance.

In order to solve the technical problems, the invention adopts the following technical scheme: the utility model provides a high-efficient collector of collecting copper, gold in follow copper smelting sediment which characterized in that: the code of the high-efficiency collector is XK-419, and the formula comprises: the compound fertilizer comprises dithiophosphate, sulfonic acid, sodium chloroacetate, xanthate, alkylamine and N, N-dimethylformamide, and the raw materials in percentage by mass are as follows: 15 to 20 percent of dithiophosphate, 15 to 25 percent of sulfonic acid, 20 to 30 percent of sodium chloroacetate, 20 to 30 percent of xanthate, 20 to 30 percent of alkylamine and 5 to 15 percent of N, N-dimethylformamide.

Preferably, the dithiophosphate is composed of at least one of dibutyl dithiophosphate, diisobutyl dithiophosphate, di-n-pentyl dithiophosphate, and diisopentyl dithiophosphate.

Preferably, the sulfonic acid is composed of at least one of taurine, benzenesulfonic acid, sulfamic acid, ethanesulfonic acid, sodium benzenesulfonate, pyridine-2-sulfonic acid.

Preferably, the xanthate is composed of at least one of sodium ethyl xanthate, sodium n-butyl xanthate, sodium isobutyl xanthate, sodium n-pentyl xanthate, sodium isopentyl xanthate, sodium sec-octyl xanthate.

Preferably, the alkylamine is composed of at least one of ethylamine, propylamine, n-butylamine, isobutylamine, n-pentylamine, isopentylamine, p-phenylenediamine, o-phenylenediamine, 1, 2-propylenediamine, 1, 6-hexamethylenediamine, 1, 4-butylenediamine, and 1, 5-naphthalenediamine.

Preferably, the mass fraction of the dithiophosphate is 15%, the mass fraction of the sulfonic acid is 15%, the mass fraction of the xanthate is 20%, the mass fraction of the sodium chloroacetate is 20%, the mass fraction of the alkylamine is 20%, and the mass fraction of the N, N-dimethylformamide is 10%.

According to the invention, more collecting agent molecules are adsorbed on the surface of the mineral by mainly utilizing the synergistic effect and the steric hindrance effect of dithiophosphate, sodium chloroacetate, xanthate and alkylamine, and the floatability of the mineral is improved. For example: the macromolecular dithiophosphate collecting agent can be selectively adsorbed on an adsorption site (formula 1) of Cu on the surface of a mineral, and the micromolecular xanthate can be adsorbed on a site of copper, a site of Fe (formula 2) and inserted between molecules of dithiophosphate. Eventually causing the mineral surface to adsorb more collector molecules. Meanwhile, the addition of dithiophosphate in the agent can improve the foaming capacity of the agent, so that more mineral particles are attached to the surface of the foam and are enriched in the concentrate. The N, N-dimethylformamide is added, so that the N, N-dimethylformamide can be adsorbed on the surface of the copper-containing mineral, the floatability of the copper-containing mineral is improved, and the medicament can be more uniformly dispersed in a pulp system, so that the molecules of the collecting agent are fully contacted with mineral particles.

(formula 1, R)1、R2Being alkyl groups)

Figure BDA0002506778510000032

(formula 2, M is Fe or Cu, R is an alkyl group)

The preparation method of the efficient collecting agent for collecting copper and gold from copper smelting slag is characterized by comprising the following steps: firstly, weighing the raw materials in proportion, then placing sodium chloroacetate in a container, adding N, N-dimethylformamide, slowly adding xanthate while stirring, and stirring and reacting in a constant-temperature water bath at 80 ℃ for 2 hours; when the temperature is reduced to 20-30 ℃, slowly dripping alkylamine into the container, and stirring for 1 hour at the constant temperature of 50 ℃; and finally, slowly adding dithiophosphate and sulfonic acid in sequence, and uniformly stirring to obtain the high-efficiency collector XK-419.

According to the invention, through utilizing the structure-activity relationship and synergistic effect among different types of collectors with different structures, molecules with stronger collecting capacity are adsorbed on adsorption sites with weaker surface activity of minerals, and molecules with weaker collecting capacity are adsorbed on adsorption sites with higher surface activity of minerals, so that more molecules of the collectors are adsorbed on the surfaces of the minerals, the high-efficiency comprehensive recovery of copper and gold in copper smelting slag is realized, the loss of valuable metals and the pollution of the valuable metals to the environment are avoided, and meanwhile, certain economic benefits can be brought to a smelting plant. Compared with the improved flotation process and equipment, the collector disclosed by the invention can be prepared by compounding common compounds, copper and gold are effectively enriched only through a simple flotation process, manpower and material resources are greatly saved, and the collector is a novel collector for efficiently recovering copper and gold from copper smelting slag at low cost.

Drawings

FIG. 1 is a one-stage open circuit flotation scheme of the present invention under laboratory conditions;

figure 2 is a flow diagram of a closed circuit flotation process under laboratory conditions according to the present invention.

Detailed Description

The invention is further illustrated by the following specific embodiments in conjunction with the accompanying drawings:

preparation of collector XK-419: firstly, weighing the raw materials in proportion, then placing sodium chloroacetate in a container, adding N, N-dimethylformamide, slowly adding xanthate while stirring, and stirring and reacting in a constant-temperature water bath at 80 ℃ for 2 hours; when the temperature is reduced to 20-30 ℃, slowly dripping alkylamine into the container, and stirring for 1 hour at the constant temperature of 50 ℃; and finally, slowly adding dithiophosphate and sulfonic acid in sequence, and uniformly stirring to obtain the high-efficiency collector XK-419.

7页详细技术资料下载
上一篇:一种医用注射器针头装配设备
下一篇:一种锂辉石矿浮选捕收剂及其制备方法、应用方法

网友询问留言

已有0条留言

还没有人留言评论。精彩留言会获得点赞!

精彩留言,会给你点赞!