Furniture coating

文档序号:1646715 发布日期:2019-12-24 浏览:20次 中文

阅读说明:本技术 一种家具涂料 (Furniture coating ) 是由 段宏伟 于 2019-08-23 设计创作,主要内容包括:本发明公开一种家具涂料,由下列重要成分混合组成,具体包括硝化棉、醇酸树脂、改性松香树脂、丙烯酸树脂、氨基树脂、二甲苯、邻苯二甲酸二丁酯、二辛酯和氧化蓖麻油。有益效果是生产成本低,附着性能强。(The invention discloses a furniture coating which is prepared by mixing the following components in parts by weight, and specifically comprises nitrocotton, alkyd resin, modified rosin resin, acrylic resin, amino resin, xylene, dibutyl phthalate, dioctyl phthalate and oxidized castor oil. The adhesive has the advantages of low production cost and strong adhesive property.)

1. The furniture coating is characterized by being prepared by mixing the following components in percentage by weight:

40-60% of nitrocotton

10-20% of alkyd resin

5 to 15 percent of modified rosin resin

5-10% of acrylic resin

1 to 5 percent of amino resin

1 to 5 percent of dimethylbenzene

Dibutyl phthalate 5-10%

5 to 10 percent of dioctyl ester

1-5% of oxidized castor oil.

2. The furniture coating according to claim 1, which is prepared by mixing the following components in percentage by weight:

50 percent of nitrocotton

Alkyd resin 12%

10 percent of modified rosin resin

Acrylic resin 8%

4 percent of amino resin

3 percent of dimethylbenzene

Dibutyl phthalate 5%

Dioctyl ester 5%

3 percent of oxidized castor oil.

Technical Field

The invention relates to a furniture coating, and belongs to the field of furniture production and manufacturing application.

Background

The existing furniture coating is deficient in the aspects of adhesion performance, production cost and the like.

Disclosure of Invention

Aiming at the problems in the prior art, the invention provides a furniture coating which is used for reducing the production cost and increasing the adhesion performance.

In order to achieve the purpose, the invention adopts the technical scheme that: a furniture coating is prepared by mixing the following components in percentage by weight:

40-60% of nitrocotton

10-20% of alkyd resin

5 to 15 percent of modified rosin resin

5-10% of acrylic resin

1 to 5 percent of amino resin

1 to 5 percent of dimethylbenzene

Dibutyl phthalate 5-10%

5 to 10 percent of dioctyl ester

1-5% of oxidized castor oil.

Further, the paint is prepared by mixing the following components in percentage by weight:

50 percent of nitrocotton

Alkyd resin 12%

10 percent of modified rosin resin

Acrylic resin 8%

4 percent of amino resin

3 percent of dimethylbenzene

Dibutyl phthalate 5%

Dioctyl ester 5%

3 percent of oxidized castor oil.

The invention has the beneficial effects that: low production cost and strong adhesion.

Detailed Description

In order to make the objects, technical solutions and advantages of the present invention more apparent, the present invention is further described in detail by examples below. It should be understood, however, that the description herein of specific embodiments is only intended to illustrate the invention and not to limit the scope of the invention.

Unless defined otherwise, all technical and scientific terms used herein have the same meaning as commonly understood by one of ordinary skill in the art to which this invention belongs, and the terms used herein in the specification of the present invention are for the purpose of describing particular embodiments only and are not intended to limit the present invention.

4页详细技术资料下载
上一篇:一种医用注射器针头装配设备
下一篇:一种仿花岗岩纯苯弹性涂层配方及制作工艺

网友询问留言

已有0条留言

还没有人留言评论。精彩留言会获得点赞!

精彩留言,会给你点赞!