Glass cover plate and electronic equipment

文档序号:1931649 发布日期:2021-12-07 浏览:25次 中文

阅读说明:本技术 一种玻璃盖板及电子设备 (Glass cover plate and electronic equipment ) 是由 周伟杰 于 2021-08-16 设计创作,主要内容包括:本发明公开了一种玻璃盖板及电子设备,其中,玻璃盖板包括,盖板本体,包括第一面和第二面,第一面的应力小于第二面,自然状态下,第一面受向内弯曲的力,第二面受向外弯曲的力,盖板本体向第一面弯曲;减反射膜,完全覆盖第二面。本发明在盖板应力大的一面镀减反射膜并再次钢化,有减反射膜的那一面由于减反射膜的阻挡而不能进行离子交换,而另外一面则进行离子交换,从而应力增加,最终达到平衡。解决了盖板弯曲的问题。便于盖板的后期加工,且提高了显示面板的整体视觉效果。(The invention discloses a glass cover plate and electronic equipment, wherein the glass cover plate comprises a cover plate body, a first side and a second side, wherein the stress of the first side is smaller than that of the second side; and the antireflection film completely covers the second surface. According to the invention, the antireflection film is plated on the surface of the cover plate with large stress and is tempered again, the surface with the antireflection film cannot perform ion exchange due to the blocking of the antireflection film, and the other surface performs ion exchange, so that the stress is increased, and the balance is finally achieved. The problem of apron crooked is solved. The later stage processing of apron is convenient for, and has improved display panel's whole visual effect.)

1. A glass cover plate is characterized by comprising,

the cover plate comprises a cover plate body and a first side, wherein the stress of the first side is smaller than that of the second side, and the cover plate body is bent towards the first side in a natural state;

and the antireflection film completely covers the second surface.

2. The glass cover plate according to claim 1, wherein the cover plate body is tempered glass.

3. The glass cover plate according to claim 1, wherein the cover plate body is tempered again after plating the antireflection film.

4. The glass cover sheet according to claim 3, wherein the antireflection film is capable of blocking ion exchange during tempering of the second side.

5. The glass cover plate according to claim 1, wherein the antireflection film is made of one or more of silicon dioxide, silicon nitride, niobium oxide, titanium oxide.

6. The glass cover plate according to claim 1, wherein said antireflection film has at least two layers.

7. The glass cover sheet according to claim 6, wherein the antireflection film has 5 to 9 layers.

8. The glass cover plate according to claim 1, wherein the antireflection film has a thickness of 200 to 500 nm.

9. The glass cover plate according to claim 1, wherein the antireflection film has a reflectivity of less than 1%.

10. An electronic device comprising the glass cover plate according to any one of claims 1 to 9.

Technical Field

The invention relates to the technical field of display panels, in particular to a glass cover plate and electronic equipment.

Background

In order to enhance the strength of the cover plate, the glass cover plate for the vehicle generally needs to be chemically toughened; as shown in fig. 1 and 2, in the flat glass 10 ', the tempering depth of the front side and the back side is often inconsistent in the chemical tempering process, and the stress of the first side 11 ' is smaller than that of the second side 12 ', so that the glass is warped. If not, the processing is not beneficial to the post processing of the glass 10', the appearance of the cover plate is affected, and even the display effect of the display panel is affected.

In view of this, there is a need to improve the existing glass cover plate to reduce the stress difference between the two sides of the cover plate after tempering.

Disclosure of Invention

The invention discloses a glass cover plate and electronic equipment, which are used for solving the problem that the cover plate warps due to the stress difference of two surfaces of the tempered cover plate in the prior art.

In order to solve the problems, the invention adopts the following technical scheme:

there is provided a glass cover plate including,

the cover plate comprises a cover plate body and a first side, wherein the stress of the first side is smaller than that of the second side, and the cover plate body is bent towards the first side in a natural state;

and the antireflection film completely covers the second surface.

In the scheme, the cover plate body is made of tempered glass.

In the scheme, the cover plate body is tempered again after being plated with the antireflection film.

In the above scheme, the antireflection film can prevent the second surface from ion exchange during tempering.

In the above aspect, the antireflection film is made of one or more of silicon dioxide, silicon nitride, niobium oxide, and titanium oxide.

In the above scheme, the antireflection film has at least two layers.

In the scheme, the antireflection film has 5-9 layers.

In the scheme, the thickness of the antireflection film is 200-500 nm.

In the above aspect, the reflectance of the antireflection film is less than 1%.

The invention also provides electronic equipment comprising the glass cover plate in any one of the above schemes.

The technical scheme adopted by the invention can achieve the following beneficial effects:

plating an antireflection film on the side of the cover plate with large stress and tempering the side again, wherein the side with the antireflection film can not carry out ion exchange due to the blocking of the antireflection film, and the other side carries out ion exchange, so that the stress is increased, and finally, the balance is achieved. The problem of apron crooked is solved. The later stage processing of apron is convenient for, and has improved display panel's whole visual effect.

Drawings

In order to more clearly illustrate the technical solutions of the embodiments of the present invention, the drawings used in the description of the embodiments will be briefly introduced below to form a part of the present invention, and the exemplary embodiments and the description thereof illustrate the present invention and do not constitute a limitation of the present invention. In the drawings:

FIG. 1 is a schematic view of a prior art non-tempered glass;

FIG. 2 is a schematic view of a prior art tempered glass;

fig. 3 is a schematic structural view of a cover plate body of a glass cover plate disclosed in embodiment 1 after an antireflection film is attached thereto;

fig. 4 is a schematic structural view of the glass cover plate disclosed in embodiment 1 of the present invention after the cover plate body is tempered again.

The following reference signs are specifically included:

prior art glass-10'; the first face-11' of the prior art; the second side-12' in the prior art; a cover plate body-10; a first side-11; a second face-12; antireflection film-20.

Detailed Description

In order to make the objects, technical solutions and advantages of the present invention more apparent, the technical solutions of the present invention will be clearly and completely described below with reference to the specific embodiments of the present invention and the accompanying drawings. It is to be understood that the described embodiments are merely exemplary of the invention, and not restrictive of the full scope of the invention. All other embodiments, which can be derived by a person skilled in the art from the embodiments given herein without making any creative effort, shall fall within the protection scope of the present invention.

As shown in fig. 3 and 4, the present invention provides a glass cover plate, including,

the cover plate comprises a cover plate body 10 and a cover plate body, wherein the cover plate body 10 comprises a first surface 11 and a second surface 12, the stress of the first surface 11 is smaller than that of the second surface 12, the first surface 11 is subjected to inward bending force in a natural state, the second surface 12 is subjected to outward bending force, and the cover plate body 10 is bent towards the first surface 11; and an antireflection film 20 completely covering the second face 20. The cover plate body 10 is made of toughened glass. And tempered again after plating the antireflection film 20. Antireflection film 20 is capable of blocking ion exchange during tempering of second face 12.

According to the invention, the second surface 12 with large stress of the cover plate body 10 is plated with the antireflection film 20 and then is tempered again, the second surface 12 cannot perform ion exchange due to the blocking of the antireflection film 20, and the first surface 11 performs ion exchange, so that the stress is increased, and finally the balance is achieved. The problem of apron crooked is solved.

The antireflection film 20 is made of one or more of silicon dioxide, silicon nitride, niobium oxide, and titanium oxide.

The antireflection film has at least two layers, and since a single layer of the antireflection film 20 hardly achieves a desired effect, a multilayer antireflection film 20 is used in order to achieve zero reflection at a single wavelength or achieve a good antireflection effect in a wide spectral region. Preferably, the antireflection film has 5 to 9 layers, and is formed by stacking two materials with different refractive indexes, wherein the low refractive index material comprises silicon dioxide, and the high refractive index material comprises silicon nitride, niobium oxide and titanium oxide.

The thickness of the antireflection film 20 is 200 to 500 nm.

In the present embodiment, the reflectance of antireflection film 20 is preferably less than 1%. The effect of eliminating the reflected light is good.

Example 2

The invention also provides an electronic device comprising the glass cover plate in the embodiment 1. The electronic equipment using the glass cover plate is characterized in that the second surface 12 with large stress of the cover plate is plated with the antireflection film 20 and is tempered again, the second surface cannot exchange ions due to the blocking of the antireflection film 20, and the first surface 11 exchanges ions, so that the stress is increased, and the balance is finally achieved. The problem of apron crooked is solved. The later stage processing of apron is convenient for, and has improved display panel's whole visual effect.

According to the invention, the antireflection film is plated on the surface of the cover plate with large stress and is tempered again, the surface with the antireflection film cannot perform ion exchange due to the blocking of the antireflection film, and the other surface performs ion exchange, so that the stress is increased, and the balance is finally achieved. The problem of apron crooked is solved. The later stage processing of apron is convenient for, and has improved display panel's whole visual effect.

While the present invention has been described with reference to the embodiments shown in the drawings, the present invention is not limited to the embodiments, which are illustrative and not restrictive, and it will be apparent to those skilled in the art that various changes and modifications can be made therein without departing from the spirit and scope of the invention as defined in the appended claims.

7页详细技术资料下载
上一篇:一种医用注射器针头装配设备
下一篇:硫系玻璃红外电磁屏蔽窗口及其制备方法

网友询问留言

已有0条留言

还没有人留言评论。精彩留言会获得点赞!

精彩留言,会给你点赞!