阅读说明:本技术 一种木板上色印刷方法 (Wood board coloring and printing method ) 是由 朱爱林 缪志良 赵彩荣 于 2018-07-06 设计创作,主要内容包括:本发明提供一种木板上色印刷方法,其特征在于,包括如下工艺步骤:1)、对木板表面进行300-500目打磨;2)、打磨完成后去掉木板表面的灰尘;3)、将底漆加热到60-78℃;4)、通过喷涂或者刷漆的方式将底漆涂装在木板表面;5)、对底漆进行烘干,烘干温度为120-140℃;6)、对烘干底漆后的木板进行上色;7)、上色后对木板表面进行透明材料封面。本发明通过打磨,打磨后上底漆,底漆烘干处理,这样可以保证底漆的稳定性,在底漆具备稳定性的基础上,颜色漆会更稳定,最后通过透明材料进行封装,使颜色漆更长久。(The invention provides a wood board coloring and printing method which is characterized by comprising the following process steps: 1) polishing the surface of the wood board by 300-500 meshes; 2) removing dust on the surface of the wood board after polishing; 3) heating the primer to 60-78 ℃; 4) coating the primer on the surface of the wood board in a spraying or painting mode; 5) drying the primer at the temperature of 120-140 ℃; 6) coloring the wood board after drying the primer; 7) and after coloring, carrying out transparent material cover on the surface of the wood board. According to the invention, the stability of the primer can be ensured by polishing, priming the ground primer and drying the primer, the color paint is more stable on the basis of the stability of the primer, and finally the color paint is longer by packaging through the transparent material.)

1. A wood board coloring and printing method is characterized by comprising the following process steps:

1) polishing the surface of the wood board by 300-500 meshes;

2) removing dust on the surface of the wood board after polishing;

3) heating the primer to 60-78 ℃;

4) coating the primer on the surface of the wood board in a spraying or painting mode;

5) drying the primer at the temperature of 120-140 ℃;

6) coloring the wood board after drying the primer;

7) and after coloring, carrying out transparent material cover on the surface of the wood board.

2. The method for coloring and printing on a wood board according to claim 1, wherein: the mesh number in the step 1) is 400 meshes.

3. The method for coloring and printing on a wood board according to claim 1, wherein: the heating temperature in the step 3) is 69 ℃.

4. The method for coloring and printing on a wood board according to claim 1, wherein: the drying temperature of the step 5) is 130 ℃.

5. The method for coloring and printing on a wood board according to claim 1, wherein: the transparent material of the step 7) is epoxy resin.

6. A method for coloring and printing a wood board according to claim 1 or 5, characterized in that: the transparent material in the step 7) is plastic with long-time scintillation.

Technical Field

The invention relates to the technical field of printing, in particular to a wood board coloring and printing method.

Background

The printing of wood boards is one of the essential processes in many industries, and the printing method is very extensive, such as the field of toys, the field of art, and the like. The existing printing method has unstable color after coloring, and is easy to fade after long-time use.

Disclosure of Invention

Technical problem to be solved

Aiming at the defects of the prior art, the invention provides the coloring and printing method for the wood board, and the coloring method can ensure that the color on the wood board is more stable and the service life is longer.

(II) technical scheme

In order to achieve the purpose, the invention provides the following technical scheme:

a wood board coloring and printing method is characterized by comprising the following process steps:

1) polishing the surface of the wood board by 300-500 meshes;

2) removing dust on the surface of the wood board after polishing;

3) heating the primer to 60-78 ℃;

4) coating the primer on the surface of the wood board in a spraying or painting mode;

5) drying the primer at the temperature of 120-140 ℃;

6) coloring the wood board after drying the primer;

7) and after coloring, carrying out transparent material cover on the surface of the wood board.

As a preferable scheme of the previous step, the mesh number in the step 1) is 400 meshes.

As a preferable scheme of the previous step, the heating temperature of the step 3) is 69 ℃.

As a preferable scheme of the previous step, the drying temperature of the step 5) is 130 ℃.

As a preferable scheme of the previous step, the transparent material in the step 7) is epoxy resin.

As a preferable scheme of the previous step, the transparent material in the step 7) is a long-flashing plastic.

(III) advantageous effects

The invention provides a wood board coloring and printing method, which has the following beneficial effects:

according to the invention, the stability of the primer can be ensured by polishing, priming the ground primer and drying the primer, the color paint is more stable on the basis of the stability of the primer, and finally the color paint is longer by packaging through the transparent material.

Detailed Description

The technical solutions in the embodiments of the present invention will be clearly and completely described below with reference to the embodiments of the present invention, and it is obvious that the described embodiments are only a part of the embodiments of the present invention, and not all of the embodiments. All other embodiments, which can be derived by a person skilled in the art from the embodiments given herein without making any creative effort, shall fall within the protection scope of the present invention.

4页详细技术资料下载
上一篇:一种医用注射器针头装配设备
下一篇:一种组框机

网友询问留言

已有0条留言

还没有人留言评论。精彩留言会获得点赞!

精彩留言,会给你点赞!