阅读说明:本技术 一种用竹草制作的家用器具方法 (Method for manufacturing household appliance by using bamboo grass ) 是由 李明 于 2021-06-23 设计创作,主要内容包括:本发明的一种用竹草制作的家用器具方法,属于家用器具编织技术领域,包括底座、腔壁、顶盖、手柄、支撑架、防水层和内衬层组成,所述底座侧壁编织有腔壁,所述腔壁顶部活动安装有顶盖,所述腔壁顶部侧壁编织有手柄,所述底座、腔壁和顶盖均为双侧结构,所述底座、腔壁和顶盖内腔均设有支撑架。本发明的有益效果是与现有技术相比,具有如下改进及优点:通过浸泡、消毒、干燥和蒸煮软化等多组加工步骤相互配合,可在对器具进行编织时,提升竹条的柔韧性,且提升竹条的耐腐蚀性,并在使用过程中减少细菌和蛀虫的产生,将有效提升器具的使用寿命等特点。(The invention discloses a method for manufacturing a household appliance by using bamboo grass, which belongs to the technical field of weaving of household appliances and comprises a base, a cavity wall, a top cover, a handle, a support frame, a waterproof layer and an inner lining layer, wherein the cavity wall is woven on the side wall of the base, the top of the cavity wall is movably provided with the top cover, the handle is woven on the side wall of the top of the cavity wall, the base, the cavity wall and the top cover are all of a bilateral structure, and the support frame is arranged in the inner cavities of the base, the cavity wall and the top cover. Compared with the prior art, the invention has the advantages that the invention has the following improvements and advantages: through soaking, disinfection, drying and boiling multiunit processing steps such as soften mutually supporting, can promote the pliability of bamboo strip when weaving the utensil, and promote the corrosion resistance of bamboo strip to reduce the production of bacterium and moth worm in the use, will effectively promote characteristics such as life of utensil.)

1. A method for manufacturing a household appliance by using bamboo grass is characterized in that: the base comprises a base, a cavity wall, a top cover, a handle, a support frame, a waterproof layer and an inner liner layer, wherein the cavity wall is woven on the side wall of the base, the top cover is movably mounted at the top of the cavity wall, the handle is woven on the side wall at the top of the cavity wall, the base, the cavity wall and the top cover are of a bilateral structure, and the support frame is arranged in the inner cavity of the base, the cavity wall and the inner cavity of the top cover.

2. The method of claim 1, wherein the method comprises the steps of: the method comprises the following steps:

s1, selecting materials and soaking: selecting high-quality bamboo strips with uniform length, width and thickness, soaking the bamboo strips in water to enable the bamboo strips to absorb enough water, so that the preservation time of the bamboo strips can be prolonged, and the flexibility of the bamboo strips can be improved by humidifying the bamboo strips to achieve the optimal weaving state;

s2, cleaning and disinfecting: placing the soaked bamboo strips into a cleaning solution for careful cleaning, and then placing the cleaned bamboo strips into a disinfectant for killing bacteria and moths on the surfaces and in the inner cavities of the bamboo strips;

s3, secondary soaking: the bamboo splints are soaked again by the chemical agent, and the liquid medicine is soaked into the inner cavity of the bamboo splints, so that the bamboo splints have corrosion resistance and antibacterial action.

S4, coloring: blending the pigment, heating and stirring the dye, and placing the bamboo strips for soaking in the pigment;

s5, drying: placing the bamboo strips in an oven for baking and heating to form a stubborn paint surface on the surfaces of the bamboo strips by the dye;

s6, cooking and softening: the bamboo strips are placed into high-temperature water liquid for cooking, so that the bamboo strips are softened, and the weaving is convenient at the later stage.

S7, knitting: weave the bamboo strip, fold into the cross with two bamboo strips earlier, then in warp direction and latitudinal direction respectively in order choosing a form of pressing one, weave horizontal 10, just form the base behind the vertical 21, when choosing a pressure, notice the distance between the adjacent bamboo strip, the form of pressing one with choosing one is bent the bamboo strip and is continued to add the bamboo strip to vertically and form the chamber wall, and will two sets of structures of weaving are put together, and weave the support frame at base, chamber wall and top cap inner chamber, base and chamber wall formula structure as an organic whole.

3. A method of manufacturing a home appliance using bamboo grass according to claim 2, wherein: the base, the cavity wall and the inner wall of the top cover are provided with waterproof layers, and the surface of each waterproof layer is provided with an inner liner layer.

4. A method of manufacturing a home appliance using bamboo grass according to claim 2, wherein: the pH value of the soaking solution is between 7.5 and 8.5, and the concentration of the disinfection solution is 1: 35 and the disinfection soaking time is 12 hours.

5. A method of manufacturing a home appliance using bamboo grass according to claim 2, wherein: the chemical agent mixture ratio of the second soaking is 80-95 parts of modified acrylic resin, 30-35 parts of polyvinyl alcohol solution, 1-5 parts of sodium polymethacrylate, 3-4 parts of ammonium persulfate, 5-8 parts of hexadecyl trimethyl ammonium chloride, 0.1-0.2 part of dodecyl dimethyl benzyl ammonium chloride, 2-2.5 parts of wetting agent, 3-3.5 parts of flatting agent, 0.10-0.15 part of defoaming agent, 0.12-0.15 part of preservative, 0.05-0.08 part of mildew preventive, 0.03-0.05 part of brightening agent, 0.02-0.04 part of terpineol and 15-26 parts of deionized water.

6. A method of manufacturing a home appliance using bamboo grass according to claim 2, wherein: the heating temperature of the pigment is between 65 and 70 degrees and the stirring speed is 30 revolutions per minute.

7. A method of manufacturing a home appliance using bamboo grass according to claim 2, wherein: the baking heating is between 60 and 63 ℃, and the baking heating time is controlled to be between 30 and 40 minutes.

8. A method of manufacturing a home appliance using bamboo grass according to claim 2, wherein: the cooking softening temperature is controlled to be 90-100 ℃, and the cooking softening time is 20 minutes.

9. A method of manufacturing a home appliance using bamboo grass according to claim 2, wherein: the thickness of the bamboo strip is 3 mm, the width of the bamboo strip is 8 mm, the length of the bamboo strip is 1500 mm, and the surface of the bamboo strip is polished by 2000-mesh abrasive paper until the surface of the bamboo strip is smooth.

Technical Field

The invention relates to the technical field of household appliance weaving, in particular to a method for manufacturing a household appliance by using bamboo grass.

Background

The bamboo weaving is a handicraft made up by using wild bamboo through the processes of cutting and splitting into thin bamboo strips or thin bamboo strips and weaving them into various utensils and handicraft articles. The craft bamboo weaving not only has great practical value, but also has deep history. Historically, the bamboo weaving industry has been in workshop form, mostly in the form of generation-to-generation transmission or in the form of workshop-to-master and apprentice relation, after apprentice learning, self-supporting, recruiting the apprentice, and orally transmitting for personal education. Generally used as daily articles and agricultural appliances. The Mount eyebrow bamboo weaving history is long, is the first national non-material cultural heritage, and is a folk process distributed in each province in south. The bamboo species in south China are rich and colorful, and about two hundred or more species of lophatherum gracile, water bamboo, Sagittaria trifoliata, Phyllostachys nigra, Phyllostachys pubescens and the like exist. The labor people use bamboo to make furniture and weave articles, and create a plurality of weaving processes with different artistic characteristics, wherein the common process comprises the following steps of 1, weaving, namely forming warp and weft interweaving by using bamboo filaments and thin bamboo strips through a picking and pressing method; 2. lathing, namely lathing the bamboo joint into a certain shape and decoration; 3. splicing, namely splicing the bamboo surface or the bamboo cross section into a flower type or a vessel; 4. stringing, namely, manufacturing bamboo joints into small sections and stringing the small sections; 5. turning over the spring, and manufacturing various vessels by using the bamboo spring.

The household appliance made of the existing bamboo grass has certain defects, the bamboo strips are woven by hands after being selected and subjected to simple processing operation, the flexibility of the bamboo strips cannot reach the optimal weaving state in the weaving process, so that the bamboo strips are easy to break in the weaving process, the woven appliance is poor in corrosion resistance in the using process, bacteria and moths are easy to breed, and the service life of the appliance is greatly shortened.

Disclosure of Invention

The invention aims to provide a method for manufacturing a household appliance by using bamboo grass, which aims to solve the problems that in the background technology, the bamboo strips are easy to break in the weaving process because the flexibility of the bamboo strips does not reach the optimal weaving state after the bamboo strips are selected and then are subjected to simple treatment operation, namely, the weaving operation is carried out by hands, the woven appliance is poor in corrosion resistance in the using process, bacteria and moths are easy to breed, and the service life of the appliance is greatly shortened.

In order to achieve the purpose, the invention adopts the technical scheme that:

the household appliance method comprises a base, a cavity wall, a top cover, a handle, a supporting frame, a waterproof layer and an inner liner layer, wherein the cavity wall is woven on the side wall of the base, the top cover is movably mounted at the top of the cavity wall, the handle is woven on the side wall at the top of the cavity wall, the base, the cavity wall and the top cover are of a bilateral structure, and the supporting frame is arranged in the inner cavity of the base, the cavity wall and the inner cavity of the top cover.

As further optimization of the technical scheme, the method is characterized in that:

the method comprises the following steps:

s1, selecting materials and soaking: selecting high-quality bamboo strips with uniform length, width and thickness, soaking the bamboo strips in water to enable the bamboo strips to absorb enough water, so that the preservation time of the bamboo strips can be prolonged, and the flexibility of the bamboo strips can be improved by humidifying the bamboo strips to achieve the optimal weaving state;

s2, cleaning and disinfecting: placing the soaked bamboo strips into a cleaning solution for careful cleaning, and then placing the cleaned bamboo strips into a disinfectant for killing bacteria and moths on the surfaces and in the inner cavities of the bamboo strips;

s3, secondary soaking: the bamboo splints are soaked again by the chemical agent, and the liquid medicine is soaked into the inner cavity of the bamboo splints, so that the bamboo splints have corrosion resistance and antibacterial action.

S4, coloring: blending the pigment, heating and stirring the dye, and placing the bamboo strips for soaking in the pigment;

s5, drying: placing the bamboo strips in an oven for baking and heating to form a stubborn paint surface on the surfaces of the bamboo strips by the dye;

s6, cooking and softening: the bamboo strips are placed into high-temperature water liquid for cooking, so that the bamboo strips are softened, and the weaving is convenient at the later stage.

S7, knitting: weave the bamboo strip, fold into the cross with two bamboo strips earlier, then in warp direction and latitudinal direction respectively in order choosing a form of pressing one, weave horizontal 10, just form the base behind the vertical 21, when choosing a pressure, notice the distance between the adjacent bamboo strip, the form of pressing one with choosing one is bent the bamboo strip and is continued to add the bamboo strip to vertically and form the chamber wall, and will two sets of structures of weaving are put together, and weave the support frame at base, chamber wall and top cap inner chamber, base and chamber wall formula structure as an organic whole.

As a further optimization of the technical scheme, waterproof layers are arranged on the base, the cavity wall and the inner wall of the top cover, and an inner lining layer is arranged on the surface of each waterproof layer.

As further optimization of the technical scheme, the pH value of the soaking solution is between 7.5 and 8.5, and the concentration of the disinfectant is 1: 35 and the disinfection soaking time is 12 hours.

As further optimization of the technical scheme, the chemical agent mixture ratio prepared by secondary soaking is 80-95 parts of modified acrylic resin, 30-35 parts of polyvinyl alcohol solution, 1-5 parts of sodium polymethacrylate, 3-4 parts of ammonium persulfate, 5-8 parts of hexadecyl trimethyl ammonium chloride, 0.1-0.2 part of dodecyl dimethyl benzyl ammonium chloride, 2-2.5 parts of wetting agent, 3-3.5 parts of flatting agent, 0.10-0.15 part of defoaming agent, 0.12-0.15 part of preservative, 0.05-0.08 part of mildew preventive, 0.03-0.05 part of brightener, 0.02-0.04 part of terpineol and 15-26 parts of deionized water.

As a further optimization of the technical scheme, the heating temperature of the pigment is between 65 and 70 ℃, and the stirring speed is 30 revolutions per minute.

As a further optimization of the technical scheme, the baking heating is between 60 and 63 ℃, and the baking heating time length is controlled to be between 30 and 40 minutes.

As further optimization of the technical scheme, the cooking softening temperature is controlled to be 90-100 ℃, and the cooking softening time is 20 minutes.

As a further optimization of the technical scheme, the thickness of the selected bamboo strips is 3 mm, the width is 8 mm, the length is 1500 mm, and the surfaces of the bamboo strips are polished by 2000-mesh sand paper until the surfaces of the bamboo strips are smooth.

The invention provides a method for manufacturing a household appliance by using bamboo grass through improvement, and compared with the prior art, the method has the following improvement and advantages: .

Detailed Description

The technical solutions in the embodiments of the present invention are clearly and completely described, and it is obvious that the described embodiments are only a part of the embodiments of the present invention, and not all embodiments. All other embodiments, which can be derived by a person skilled in the art from the embodiments given herein without making any creative effort, shall fall within the protection scope of the present invention.

The household appliance method comprises a base, a cavity wall, a top cover, a handle, a supporting frame, a waterproof layer and an inner liner layer, wherein the cavity wall is woven on the side wall of the base, the top cover is movably mounted at the top of the cavity wall, the handle is woven on the side wall at the top of the cavity wall, the base, the cavity wall and the top cover are of a bilateral structure, and the supporting frame is arranged in the inner cavity of the base, the cavity wall and the inner cavity of the top cover.

As further optimization of the technical scheme, the method comprises the following steps:

s1, selecting materials and soaking: selecting high-quality bamboo strips with uniform length, width and thickness, soaking the bamboo strips in water to enable the bamboo strips to absorb enough water, so that the preservation time of the bamboo strips can be prolonged, and the flexibility of the bamboo strips can be improved by humidifying the bamboo strips to achieve the optimal weaving state;

s2, cleaning and disinfecting: placing the soaked bamboo strips into a cleaning solution for careful cleaning, and then placing the cleaned bamboo strips into a disinfectant for killing bacteria and moths on the surfaces and in the inner cavities of the bamboo strips;

s3, secondary soaking: the bamboo splints are soaked again by the chemical agent, and the liquid medicine is soaked into the inner cavity of the bamboo splints, so that the bamboo splints have corrosion resistance and antibacterial action.

S4, coloring: blending the pigment, heating and stirring the dye, and placing the bamboo strips for soaking in the pigment;

s5, drying: placing the bamboo strips in an oven for baking and heating to form a stubborn paint surface on the surfaces of the bamboo strips by the dye;

s6, cooking and softening: the bamboo strips are placed into high-temperature water liquid for cooking, so that the bamboo strips are softened, and the weaving is convenient at the later stage.

S7, knitting: weave the bamboo strip, fold into the cross with two bamboo strips earlier, then in warp direction and latitudinal direction respectively in order choosing a form of pressing one, weave horizontal 10, just form the base behind the vertical 21, when choosing a pressure, notice the distance between the adjacent bamboo strip, the form of pressing one with choosing one is bent the bamboo strip and is continued to add the bamboo strip to vertically and form the chamber wall, and will two sets of structures of weaving are put together, and weave the support frame at base, chamber wall and top cap inner chamber, base and chamber wall formula structure as an organic whole.

As a further optimization of the technical scheme, waterproof layers are arranged on the base, the cavity wall and the inner wall of the top cover, and an inner lining layer is arranged on the surface of each waterproof layer.

As further optimization of the technical scheme, the pH value of the soaking solution is between 7.5 and 8.5, and the concentration of the disinfectant is 1: 35 and the disinfection soaking time is 12 hours.

As further optimization of the technical scheme, the chemical agent mixture ratio prepared by secondary soaking is 80-95 parts of modified acrylic resin, 30-35 parts of polyvinyl alcohol solution, 1-5 parts of sodium polymethacrylate, 3-4 parts of ammonium persulfate, 5-8 parts of hexadecyl trimethyl ammonium chloride, 0.1-0.2 part of dodecyl dimethyl benzyl ammonium chloride, 2-2.5 parts of wetting agent, 3-3.5 parts of flatting agent, 0.10-0.15 part of defoaming agent, 0.12-0.15 part of preservative, 0.05-0.08 part of mildew preventive, 0.03-0.05 part of brightener, 0.02-0.04 part of terpineol and 15-26 parts of deionized water.

As a further optimization of the technical scheme, the heating temperature of the pigment is between 65 and 70 ℃, and the stirring speed is 30 revolutions per minute.

As a further optimization of the technical scheme, the baking heating is between 60 and 63 ℃, and the baking heating time length is controlled to be between 30 and 40 minutes.

As further optimization of the technical scheme, the cooking softening temperature is controlled to be 90-100 ℃, and the cooking softening time is 20 minutes.

As a further optimization of the technical scheme, the thickness of the selected bamboo strips is 3 mm, the width is 8 mm, the length is 1500 mm, and the surfaces of the bamboo strips are polished by 2000-mesh sand paper until the surfaces of the bamboo strips are smooth.

The previous description of the disclosed embodiments is provided to enable any person skilled in the art to make or use the present invention. Various modifications to these embodiments will be readily apparent to those skilled in the art, and the generic principles defined herein may be applied to other embodiments without departing from the spirit or scope of the invention. Thus, the present invention is not intended to be limited to the embodiments shown herein but is to be accorded the widest scope consistent with the principles and novel features disclosed herein.

6页详细技术资料下载