具有良好耐腐蚀性和高拉伸强度的镍合金以及制造半成品的方法
阅读说明:本技术 具有良好耐腐蚀性和高拉伸强度的镍合金以及制造半成品的方法 (Nickel alloy with good corrosion resistance and high tensile strength and method for producing semi-finished product ) 是由 J·柏提娜 B·格尔曼 H·奥福斯 于 2020-03-17 设计创作,主要内容包括:本发明涉及镍合金,其包含(以重量%计)Ni 50-55%,Cr 17-21%,Mo>0-9%,W 0-9%,Nb 1-5.7%,Ta>0-4.7%,Ti>0.1-3.0%,Al 0.4-4.0%,Co最大3.0%,Mn最大0.35%,Si最大0.35%,Cu最大0.23%,C 0.001-0.045%,S最大0.01%,P 0.001-0.02%,B 0.001-0.01%,余量由Fe和常规工艺相关的杂质组成,其中满足下列关系:Nb+Ta 1-5.7%(1),Al+Ti>1.2-5%(2),Mo+W3-9%(3),其中Nb、Ta、Al和Ti是所涉及元素以重量%计的浓度。(The invention relates to a nickel alloy comprising (in% by weight) Ni 50-55%, Cr 17-21%, Mo > 0-9%, W0-9%, Nb 1-5.7%, Ta > 0-4.7%, Ti > 0.1-3.0%, Al 0.4-4.0%, Co max 3.0%, Mn max 0.35%, Si max 0.35%, Cu max 0.23%, C0.001-0.045%, S max 0.01%, P0.001-0.02%, B0.001-0.01%, the balance consisting of Fe and impurities associated with conventional processes, wherein the following relationships are satisfied: nb + Ta 1-5.7% (1), Al + Ti > 1.2-5% (2), Mo + W3-9% (3), wherein Nb, Ta, Al and Ti are the concentrations of the elements involved in weight%.)